Describe the conduct of a typical creep test

Answer & Explanation Solved by verified expert
4.1 Ratings (482 Votes)
A Creep test measures th pressure rate of deformationof a given material at high temperatures Creep test is conducted using a tensile specimen to which a contant stress is applied at constant temperature to a constant load and recording the    See Answer